Firing temperature : cone 10 | Surface texture : satin | Color : clear | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Apply thin by dipping or pouring in and out if just used as liner, and fire to cone 10 in a wood kiln with heavy reduction. I use this glaze to show iff brushwork underneath. Fly ash from a wood firing has little effect on this glaze.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.