Amber’s Gongshow

Amber’s Gongshow

Firing temperature : cone 10 | Surface texture : glossy | Color : clear | Atmosphere: Reduction

Published in "High-Fire Celadons" by Adam Field, in the March 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions