Firing temperature : cone 10 | Surface texture : matte | Color : white | Atmosphere: Reduction

This recipe was published in the June/July/August 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Mix borax separately with hot water and add to the wet glaze mix, then sieve. I mix this slip to a heavy cream consistency. For use on bisque ware. I bisque fire to cone 08. Glaze can be applied over the slip.