Ceramic Recipes logo

Wash

Wash

Firing temperature : cone 04-10 | Color : various | Atmosphere: Oxidation/Neutral Reduction

Published in "Low-Fire Glazes" by Lauren Karle, in the October 2016 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Mix by volume. This wash give you more intense colors than adding Mason stains to slip. You do not need to add deflocculant to the wash.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend