Vince Patella All Temperature Slip

Firing temperature : cone 04-10 | Surface texture : matte | Color : various | Atmosphere: Oxidation/Neutral Reduction

Published in "Emerging Artist Recipes" in the May 2017 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

I decorate at the leather-hard stage using Amaco Velvet Underglazes and newspaper resist (most of this is laser cut). Once the underglaze color is down, I then apply a layer of white slip over it. I mix the slip without the Zircopax so that it is a bit transparent and the colors come through.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend