Robert Briscoe’s White Bisque Slip

Robert Briscoe’s White Bisque Slip

Firing temperature : cone 9-10 | Atmosphere: Oxidation/Neutral Reduction

Published in "Cone 10 Clay & Glazes" by Robert Briscoe, in the Oct 2015 issue of Ceramics Monthly.

High-fire slip to use on bisque ware. The image shown here is Robert Briscoe's White Bisque Slip underneath White Ash Glaze.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Do not make substitutions for the Georgia Kaolin. Use in a half-and-half cream consistency applied in layers for a crackle surface. I use this slip to mask out iron in my stoneware and to change the glaze colors.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend