Firing temperature : cone 04-10 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral Reduction

White to toasty brown/orange in a cone 6 soda firing. Works well in a wide temperature range in oxidation and reduction.

Published in "Low-Fire Surfaces" by Ronan Kyle Peterson, in the September 2017 issue of Ceramics Monthly.

Click Image to Enlarge


I apply one coat of Oestreich White Slip using dipping or pouring methods.