Iron Oxide Slip

Iron Oxide Slip

Firing temperature : cone 10 | Surface texture : satin matte | Color : brown | Atmosphere: Oxidation Reduction

This recipe was contributed by Elena Renker in the November 2019 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

I add Sussett (Peptapon #52) to this slip for better brushability. Sussett is an organic gum powder (like CMC Gum) that is mixed with boiling water in a ratio of 20g powder to 1 quart (1L) water. It forms a gel that can be mixed with glazes. Add 4 tsp. (20 mL) of Sussett gel per 1 quart (1L) of glaze.