Green Egyptian Paste

Firing temperature : cone 016 | Surface texture : matte | Color : light green | Atmosphere: Oxidation/Neutral

Published in "Egyptian Paste" by Robin Hopper, in the Jul/Aug 2010 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

Mix well and sieve to 60-mesh or finer while dry. Add a small amount of water and mix to a dough-like consistency.