Firing temperature : cone 7 | Surface texture : matte to satin | Color : light brown | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Mix to a specific gravity of 1.3 for dipping or 1.4 for brushing. When testing kaolins for this slip, 6 Tile Kaolin, EPK Kaolin, or Helmer Kaolin work best.

This recipe was shared by Nathan Willever in the May 2019 Ceramics Monthly.