Firing temperature : cone 05 | Surface texture : matte | Color : black | Atmosphere: Oxidation/Neutral

Published in "Push/Pull: The Art of Deborah Sigel" by Mary Cloonan, in the Mar/Apr 2014 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Mixing: Start with 33% water as each colorant takes a different amount of water, cobalt carbonate needing a good bit more than the others. Add more water in smaller increments as the paste can quickly become over hydrated and sticky. Paste tends to stiffen up by the next day or two and will need to be re-wedged to become pliable again.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend