Black Wash/Stain
Firing temperature : cone 10-11 | Color : black | Atmosphere: Oxidation/Neutral ReductionPublished in "Wood/soda-fired recipes," in the April 2016 issue of Ceramics Monthly, page 62.
Ingredients
- 16.46
- 16.45
- 16.45
- 25.32
- 25.32
Instructions
Mix and apply the Black Wash/Stain thin, like water color. To accentuate relief textures on the surface of pieces, after the wash dries, use a damp sponge to remove it from high points.