Firing temperature : cone 04-10 | Color : white | Atmosphere: Oxidation/Neutral Reduction

Published in "Slippery When Wet" by Jason Bige Burnett, in the Sep/Oct 2011 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

*Mason stain percentages vary per color. Try testing within the range of 3-10% to start.