Val Cushing Floor Tile Body

Val Cushing Floor Tile Body

Firing temperature : Cone 6 | Color : off white | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

This is a very durable and highly vitrified off white tile body. The molochite helps to mitigate warping, but is not 100% necessary.

This recipe was shared by Forrest Lesch-Middelton in the October 2020 issue of Ceramics Monthly.