Tangerine Trip (Orange Porcelain)

Color : Orange | Atmosphere: Oxidation/Neutral Reduction

Published in "Pour It On! Recipes" by Carly Van Anglen and David Ferro, Alina Hayes, and Justin Donofrio in the September 2017 issue of Ceramics Monthly.

 


Click Image to Enlarge

Instructions

To mix, start with a slurry of porcelain base (I use the two commercially available porcelain bodies listed above) and slowly add stain mixture. Dry to desired consistency on plaster slabs. In oxidation, fire to lower temperature for a creamy orange, fire to high temperature for a more saturated tone. Stains can be used with any porcelain; reclaim makes a great base.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend