Severson Special Stoneware Clay Mix

Firing temperature : cone 10 | Surface texture : matte | Color : tan | Atmosphere: Reduction

This clay works well for wheel throwing and for making wheel-thrown and altered forms.

This recipe was published in the June/July/August 2018 issue of Ceramics Monthly.


Click Image to Enlarge