Seth’s Iron-Rich Stoneware #1

Seth's Iron-Rich Stoneware #1

Firing temperature : cone 6-8 | Surface texture : matte | Color : brown | Atmosphere: Reduction

Click Image to Enlarge

Instructions

This stoneware recipe was developed to be very open handbuilding clay bodies with the addition of sand or grog to taste. For wheel throwing, run through a de-airing pugmill for added plasticity.

For the best color response for all 4 recipes, fire in a wood-burning kiln with moderate to heavy reduction. After soaking at peak temperature, cool the kiln in reduction to between 1450°–1650°F. For brighter reds, cool to 1575°–1650°F. For darker blacks and purples, cool to 1450°–1550°F.

This recipe was shared by Seth Charles in the March 2021 issue of Ceramics Monthly. 

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend