Ron Meyer’s Lowfire Salt #1

Firing temperature : cone 04 | Color : dark red | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This clay body functions well for both wheel throwing and handbuilding. It darkens significantly in a salt firing.

This recipe was shared by Mike Cinelli in the March 2019 issue of Ceramics Monthly.