Ceramic Recipes logo

Rado Red Stoneware

Firing temperature : cone 5-8 | Color : brown | Atmosphere: Oxidation/Neutral

Smooth and strong red stoneware for throwing and handbuilding.

Published in "Pour It On! Recipes" by Carly Van Anglen and David Ferro, Alina Hayes, and Justin Donofrio in the September 2017 issue of Ceramics Monthly


Click Image to Enlarge

Instructions

Oxidation only. Toasty iron red in salt/soda atmospheres. Higher temperature darkens toward brown, lower temperature preserves red color.