Parian Test 9

Parian Test 9

Firing temperature : cone 9 | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

Considerably more translucent with a yellowish hue. Pleasant matte self-glazing sheen, fired to cone 9.

This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.