Parian Test 1
Firing temperature : cone 9 | Color : white | Atmosphere: Oxidation ReductionIngredients
- 40
- 20
- 40
Instructions
Very white with sufficient translucency. Sample is fairly stable in the cone-9 firing. Not enough self glazing on the surface.
This recipe was shared by Antoinette Badenhorst in the November 2020 issue of Ceramics Monthly.