Ceramic Recipes logo

Orange Earthenware

Orange Earthenware

Firing temperature : cone 04 | Color : orange-red-brown | Atmosphere: Oxidation/Neutral

Published in "Low-Fire Glazes" by Lauren Karle, in the October 2016 issue of Ceramics Monthly.

The clay body can be seen on the rim of the bowl in the image shown on this page.


Click Image to Enlarge

Instructions

To prevent scumming on the surface of the fired clay body, add 1/4 cup barium carbonate for every 100 pounds of dry clay. Dissolve the barium carbonate in hot water first, then add the dry ingredients to the wet.