Firing temperature : Cone 6 | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Mix Veegum T and bentonite separately with warm water. Mix casting slip to specific gravity of 1.6.

This recipe was shared by Jacob Monroe in the May 2021 issue of Ceramics Monthly.