Matt Schiemann’s Clay Body

Matt Schiemann’s Clay Body

Firing temperature : cone 10 | Surface texture : matte | Color : medium tan | Atmosphere: Oxidation/Neutral Reduction Wood

Published in "Woodfire Glazes" by Matt Schiemann, in the Jan 2014 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

This clay body works well in wood fired kilns. Helmar Kaolin is added to increase the flashing response of the clay when exposed to the wood-kiln atmosphere.