Mason-Stained Porcelain

Mason-Stained Porcelain

Firing temperature : Cone 6 | Atmosphere: Oxidation

This recipe was shared in "Milk + Cookies" by Adrienne Eliades in the November/December 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Ingredients

Instructions

For 1 lb of clay, use 3–5 tsp of Mason stain.

Wearing gloves, form a ball of clay into a small pinch pot. Add the powdered stain inside the pot. Then knead until the mixture is completely homogenized.