Firing temperature : Cone 6 | Atmosphere: Oxidation

This recipe was shared in "Milk + Cookies" by Adrienne Eliades in the November/December 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Ingredients

Instructions

For 1 ltr. of casting slip, use 8 tsp. of Mason stain.

Add stain to casting slip and blunge well with an immersion blender. Then sieve mixture through an 80-mesh sieve. My favorite Mason stains are Mango, Robin;s Egg, Bermuda, Best Black, and Canary.