Ceramic Recipes logo

Mason-Stained Porcelain

Mason-Stained Porcelain

Firing temperature : cone 7 | Color : various | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

*Use 3–5 tsp Mason stain per pound of clay.

Wearing gloves, form the ball of clay into a small pinch pot. Add the powdered stain inside the pot. Then knead or wedge until mixture is completely homogenized. Vary the amount of the Mason stain used based on the desired saturation.

This recipe was shared by Adrienne Eliades in the September/October 2021 issue of Pottery Making Illustrated.