Lisa Naples Earthenware Clay
Firing temperature : cone 1–2 | Color : terra cotta | Atmosphere: OxidationIngredients
- 4.04
- 7.07
- 3.03
- 10.10
- 65.66
- 10.10
- 0.51
- 1.01
Add:
Instructions
Add barium carbonate to prevent scumming.
This recipe was shared by Lisa Naples in the November 2020 issue of Ceramics Monthly.