Firing temperature : cone 04 | Atmosphere:

Published in "Cone 04 Clay & Glaze" by Mark Pharis, in the Nov 2015 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

The barium carbonate is added to reduce scumming on the surface of the fired clay body.