Firing temperature : Cone 6 |
Surface texture : matte |
Color : white |
Atmosphere:
Oxidation
Ingredients
- 1
- 9
- 35
- 23
- 25
- 7
- 42
- 0.25
Add:
Instructions
Add up to 0.5% sodium silicate. This is a modified Hensely/Polseno recipe. It fires to a warm white and works well for casting complicated forms.
This recipe was shared by Shalene Valenzuela in the March 2019 issue of Ceramics Monthly.