Cone 04 Casting Body

Firing temperature : cone 04 | Surface texture : matte | Color : white | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Sturdy earthenware body that fires white at cone 04.

This recipe was shared by Shalene Valenzuela in the March 2019 issue of Ceramics Monthly.