Firing temperature : Cone 6 |
Surface texture : satin matte |
Color : pink |
Atmosphere:
Oxidation/Neutral
Originally published in the May 2018 issue of Ceramics Monthly.
Ingredients
Instructions
Rose Pink Stain Mix: 75% Mason Stain #6020 and 25% Mason Stain #6318.
Start with adding 5% for Rose Pink. With Laguna Glacier Slip I can use a lower percentage of stain mix. When mixing my own casting slip, I generally double the amount of stain.