Coleman’s Porcelain (Revised)

Coleman's Porcelain (Revised)

Firing temperature : cone 10-11 | Color : white | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Also add 1 tsp of CMC gum per 220-pound batch.

Mix bentonite separately, and mix other materials in order from dense to light particles. Mahavir feldspar is a replacement for G200 feldspar.

This is a vitreous, translucent clay body that is excellent all around and has great green strength. This clay body begins to slump and warp from cone 11–12.

Add 0.3% Darvan 7 to the slurry to create a casting slip.

This recipe was shared by Jacob Monroe in the May 2021 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend