Bomb-Proof White Tile Body

Bomb-Proof White Tile Body

Firing temperature : cone 10 | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

This recipe limits warping, and works very well when extruded, rolled, or pressed (it also throws like a dream). It fires to white with a yellow hue in oxidation, and white with a blue hue in reduction.

This recipe was shared by Forrest Lesch-Middelton in the October 2020 issue of Ceramics Monthly.