Firing temperature : cone 10 | Surface texture : glossy | Color : black | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

I layer this black underglaze under Seafoam Green glaze, but it is a great black all by itself. Fire to cone 10 in reduction in a gas kiln.

This recipe was shared by Mark Cortright in the October 2021 issue of Ceramics Monthly.