White Slip

Firing temperature : cone 10 | Surface texture : matte | Color : white | Atmosphere: Reduction

Originally published in the May 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Ingredients

Instructions

Mix the slip to a thicker consistency, then add water to your preference. For slip trailing application, fill slip trailing bottle with thick slip and add water as needed.