White Slip
Firing temperature : cone 04-10 | Surface texture : matte | Color : white | Atmosphere: Oxidation ReductionIngredients
- 25
- 25
- 25
Instructions
If applied to bone-dry ware by brushing, a fine crackle pattern can appear in the surface of the slip.
This recipe was shared by Mike Gesiakowskiin the July/August 2019 issue of Pottery Making Illustrated.