Firing temperature : cone 04-11 | Surface texture : matte to satin | Color : Orange | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

I mix these terra sigillata recipes in 1000 gram batches, which require 8 cups of water. To make the mixing easier, I use wide mouth gallon jugs, and prefer glass so it is easier to see whether the layers have separated.

Making Terra Sigillatas

Mix deflocculent (I use sodium hexametaphosphate, a fabric water softener from the Dharma Trading Company) in warm water, preferably in a blender, pour into a container with correct quantity of water and add dry materials. After sieving, ball mill the terra sigillata 6–8 hours to increase the amount produced in a measured batch and reduce waste. After ball milling, let the terra sigillata settle for a week or more in a clear container, ladle off the clear water layer on top, then pour off the middle layer of terra sigillata. A layer of larger clay particles will have settled on the bottom of the container.

This recipe was shared by Alan Willoughby in the April 2019 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend