Firing temperature : cone 04-2 | Surface texture : satin | Color : gray | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Add 0.25–0.5% deflocculant.

The deflocculant percentage is based on the dry weight of the clay. This recipe was adapted from Pete Pinnell's Easy Terra Sigillata. The measurements for the following color suggestions are inspired by Marty Fielding's terra sigillata recipe and are based on using 1 cup of liquid Grolleg base terra sigillata.

For Gray, add between 1–6 tsp.

This recipe was shared by Rhonda Willers in the July/August 2019 issue of Pottery Making Illustrated.

 

 

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend