Rhonda’s Blue/Black Terra Sigillata

Rhonda's Blue/Black Terra Sigillata

Firing temperature : cone 04-10 | Surface texture : satin | Color : black | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Measurements for colorants are per 8 oz/1 cup liquid terra sigillata. This recipe has a great range and even works well in a wood kiln.

This recipe was shared by Rhonda Willers in the June/July 2020 issue of Pottery Making Illustrated.