Firing temperature : cone 8-11 | Surface texture : glossy | Color : brown | Atmosphere: Reduction

Click Image to Enlarge

Instructions

Apply very thinly on greenware or bisque ware. Slip can be dipped or sprayed. Always apply the slip first before applying glaze.

This recipe was shared by Andrew McIntyre in the April 2019 issue of Ceramics Monthly.