Firing temperature : cone 04-10 | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

This slip can be applied in various consistencies. I add water and mix until it achieves a creamy, milkshake thickness. I apply two coats for an opaque background on my forms. This slip fits any clay body from low fire to high fire.

This recipe was shared by Sara Ballek in the November/December 2020 issue of Pottery Making Illustrated.