Ceramic Recipes logo

Pink Slip

Pink Slip

Firing temperature : cone 9 | Surface texture : satin | Color : pink | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

The slip base used for the pink also works with other stains, so allow yourself to experiment. Its application can be rather thick, about the consistency of heavy cream. Use any transparent glaze to finish.

This recipe was shared by Jason Hartsoe in the September/October 2021 issue of Pottery Making Illustrated.