Pete’s Forgiving White Slip

Firing temperature : cone 04 | Surface texture : satin matte | Color : white | Atmosphere: Oxidation/Neutral

Published in "Deep Plates" by Kristin Pavelka, in the Sep/Oct 2011 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Can be applied to leather-hard, bone dry, or bisqued clay.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • I mixed a batch of Pete’s forgiving white slip. Is it supposed to look white when you apply it or does it turn white after firing? My batch is not white. Thanks