Ostrom’s White Slip

Firing temperature : cone 04 | Surface texture : satin matte | Color : white | Atmosphere: Oxidation/Neutral

Published in "Throw, Cut and Paste" by Joan Bruneau, in the Nov/Dec 2010 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

For use with wet to leather-hard clay.