Firing temperature : cone 02 | Surface texture : matte | Color : white | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

I mix this slip to a thick sour cream consistency for use on my work. I apply it to the back of my underglaze transfer stickers, using it both as a background for the illustrations and to adhere the transfers to the pots. I also apply this slip directly to the pieces to enhance texture.

This recipe was shared by Arthur Halvorsen in the the September 2019 issue of Ceramics Monthly.