Low Fire White Engobe (Gail Kendall)

Low Fire White Engobe (Gail Kendall)

Firing temperature : cone 06-03 | Surface texture : satin matte | Color : white | Atmosphere: Oxidation/Neutral Reduction

Shared by Lisa Pedolsky. Originally published in the Nov/Dec issue of Pottery Making Illustrated.

 


Click Image to Enlarge

Ingredients

Instructions

Mix to the consistency of heavy cream. Brush on 2–3 coats.