Firing temperature : cone 06–13 | Surface texture : satin | Color : black | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Measurements in parts.

Use a brayer to evenly roll a coat of the ink mixture onto photocopied designs (sealed in gum arabic) for a lithographic transfer process. If firing to cone 06, apply a glaze over the stain otherwise it can be rubbed off. I normally fire to cone 10 in reduction.

This recipe was shared by Mark Chuck in the June/July/August 2019 issue of Ceramics Monthly.