Line Blend Recipe 3
Firing temperature : cone 3 | Surface texture : satin | Color : Orange | Atmosphere: Oxidation SodaIngredients
- 22.0
- 62.5
- 15.5
Instructions
This recipe was shared by Katie Fee in the March 2021 issue of Ceramics Monthly.