Laterite Slip
Firing temperature : cone 5–10 | Surface texture : matte | Color : brown | Atmosphere: ReductionIngredients
- 100
Instructions
Mix to a light cream consistency and apply at stiff leather hard. Can be thinned to skim-milk consistency and applied to bisque ware. Slip can be dipped, poured, or brushed. I prefer to brush on multiple coats with overlapping brushstrokes.
This recipe was shared by Seth Charles in the March 2021 issue of Ceramics Monthly.